Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 1000 - 2500 hour | 1000 - 2500 hour | Average value: 1560 hour Grade Count:6 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |