Polymer Property : Environmental Stress Crack Resistance = 240 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 240 hour
240 hour
Condition B, 10%; ASTM D1693
ExxonMobil LL 6407.67 Injection Molding Resin
L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa..