Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 24.0 - 24.0 hour @Temperature 50.0 - 50.0 °C |
24.0 - 24.0 hour @Temperature 122 - 122 °F |
Average value: 1000 hour Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Environmental Stress Crack Resistance | 24.0 - 1000 hour | 24.0 - 1000 hour | Average value: 522 hour Grade Count:32 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |