Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 192 hour | >= 192 hour | Condition C, F0, 100% Igepal; ASTM D1693 |
Ineos TC46-25 HDPE TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-.. |