Polymer Property : Environmental Stress Crack Resistance = 15000 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance >= 15000 hour

@Temperature 50.0 - 50.0 °C
>= 15000 hour

@Temperature 122 - 122 °F
Average value: 15000 hour Grade Count:3
Overview of materials for Polybutene
This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..