Polymer Property : Environmental Stress Crack Resistance = 15.0 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 15.0 - 1000 hour

@Temperature 50.0 - 60.0 °C
15.0 - 1000 hour

@Temperature 122 - 140 °F
Average value: 240 hour Grade Count:20
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..