Environmental Stress Crack Resistance 13.0 - 530 hour

@Temperature 40.0 - 50.0 °C
13.0 - 530 hour

@Temperature 104 - 122 °F
Average value: 240 hour Grade Count:15
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Environmental Stress Crack Resistance 13.0 - 530 hour

@Thickness 1.90 - 2.00 mm
13.0 - 530 hour

@Thickness 0.0748 - 0.0787 in
Average value: 240 hour Grade Count:15
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..