Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 1.00 - 1.00 hour @Temperature 50.0 - 50.0 °C |
1.00 - 1.00 hour @Temperature 122 - 122 °F |
Average value: 1.00 hour Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Environmental Stress Crack Resistance | 1.00 - 1.00 hour @Thickness 2.00 - 2.00 mm |
1.00 - 1.00 hour @Thickness 0.0787 - 0.0787 in |
Average value: 1.00 hour Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |