Physical Properties Metric English Comments
Oxygen Transmission Rate 850 cc/m²/day

@Temperature 23.0 °C
54.8 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB666 OPP Film
Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Oxygen Transmission Rate 850 cc/m²/day

@Temperature 23.0 °C
54.8 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low seal temperature (VLTS) coating. VLTS coating provides excellent perf..
Oxygen Transmission Rate 850 cc/m²/day

@Temperature 23.0 °C
54.8 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 25MBT666 OPP Film
Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant..
Oxygen Transmission Rate 850 cc/m²/day

@Temperature 23.0 °C
54.8 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 26MB600 OPP Film
Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia..