Polymer Property : Oxygen Transmission Rate = 65.0 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 1010 cc/m²/day

@Temperature 23.0 °C
65.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB666 OPP Film
Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos..
Oxygen Transmission Rate 1010 cc/m²/day

@Temperature 23.0 °C
65.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MB668 OPP Film
Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid..
Oxygen Transmission Rate 1010 cc/m²/day

@Temperature 23.0 °C
65.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel..
Oxygen Transmission Rate 1010 cc/m²/day

@Temperature 23.0 °C
65.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 20MBT666 OPP Film
Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as..