Polymer Property : Oxygen Transmission Rate = 601 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 601 cc/m²/day

@Temperature 23.0 °C
38.7 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 40MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea..
Oxygen Transmission Rate 601 cc/m²/day

@Temperature 23.0 °C
38.7 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Bicor™ 40MB668 OPP Film
Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo..