Oxygen Transmission Rate 2300 cc/m²/day

@Thickness 0.120 mm,
Temperature 21.0 °C
148 cc/100 in²/day

@Thickness 0.00472 in,
Temperature 69.8 °F
ASTM D3985
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE)
Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer..