Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 202 cc/m²/day @Temperature 23.0 °C |
13.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |