Oxygen Transmission Rate 100 cc/m²/day

@Temperature 23.0 °C
6.45 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Metallyte™ 20MM480 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. It is typically used in lamination with other substrates on HFFS and V..