Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.35 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.43 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Oxygen Transmission | 1.35 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.43 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Oxygen Transmission | 1.35 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.43 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |