Oxygen Transmission 84.4 - 96.0 cc-mm/m²-24hr-atm
214 - 244 cc-mil/100 in²-24hr-atm
0% RH
BiologiQ ESR-PE EcoStarch mLLDPE Blend
Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ