Physical Properties Metric English Comments
Oxygen Transmission 348 cc-mm/m²-24hr-atm
884 cc-mil/100 in²-24hr-atm
or 18300 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista..