Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.720 - 236 cc-mm/m²-24hr-atm | 1.83 - 599 cc-mil/100 in²-24hr-atm | Average value: 205 cc-mm/m²-24hr-atm Grade Count:20 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |