Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 230 cc-mm/m²-24hr-atm | 584 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |