Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 55.0 cc-mm/m²-24hr-atm | 140 cc-mil/100 in²-24hr-atm | or 2200 cc/m²-atm-24 hr per 25 µm film; 38°C; 90% RH Difference |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |