Oxygen Transmission 1.77 - 138 cc-mm/m²-24hr-atm
4.49 - 351 cc-mil/100 in²-24hr-atm
Average value: 59.8 cc-mm/m²-24hr-atm Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..