Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 118 cc-mm/m²-24hr-atm | 300 cc-mil/100 in²-24hr-atm | |
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries. |