Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 3.60 cc-mm/m²-24hr-atm
9.14 cc-mil/100 in²-24hr-atm
or 47 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used..