Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.350 - 3.50 cc-mm/m²-24hr-atm
0.889 - 8.89 cc-mil/100 in²-24hr-atm
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by..