Polymer Property : Oxygen Transmission = 264 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 264 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
671 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
film; ASTM D3985
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..