Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
25 µm film; ASTM D1434-82; 50% RH
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
25 µm film; ASTM D1434-82; 50% RH
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
25 µm film; ASTM D1434-82; 50% RH
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).Genera..
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
25 µm film; ASTM D1434-82; 50% RH
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
25 µm film; ASTM D1434-82; 50% RH
DuPont™ Kapton® 200HN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General ..
Oxygen Transmission 9.90 cc-mm/m²-24hr-atm
25.1 cc-mil/100 in²-24hr-atm
Average value: 9.90 cc-mm/m²-24hr-atm Grade Count:5
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..