Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 150 cc-mm/m²-24hr-atm @Thickness 0.120 mm, Temperature 21.0 °C |
381 cc-mil/100 in²-24hr-atm @Thickness 0.00472 in, Temperature 69.8 °F |
ASTM D3985 |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Oxygen Transmission | 150 cc-mm/m²-24hr-atm | 381 cc-mil/100 in²-24hr-atm | |
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Oxygen Transmission | 150 cc-mm/m²-24hr-atm | 381 cc-mil/100 in²-24hr-atm | |
3M Dyneon™ Aflas® FA-150E PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Oxygen Transmission | 150 cc-mm/m²-24hr-atm | 381 cc-mil/100 in²-24hr-atm | |
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Oxygen Transmission | 150 cc-mm/m²-24hr-atm | 381 cc-mil/100 in²-24hr-atm | |
3M Dyneon™ Aflas® FA-150P PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Oxygen Transmission | 150 cc-mm/m²-24hr-atm | 381 cc-mil/100 in²-24hr-atm | |
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |