Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 138 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
350 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
ASTM D1434 |
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf.. |
|||
Oxygen Transmission | 138 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
350 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
ASTM D1434 |
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System Information provided by Reltek LLC |
|||
Oxygen Transmission | 138 cc-mm/m²-24hr-atm | 351 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin