Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 12.0 cc-mm/m²-24hr-atm | 30.5 cc-mil/100 in²-24hr-atm | 42% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant. |
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer 42% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |