Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 470 cc-mm/m²-24hr-atm @Thickness 1.90 mm, Temperature 21.0 °C |
1190 cc-mil/100 in²-24hr-atm @Thickness 0.0748 in, Temperature 69.8 °F |
ASTM D3985 |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |