Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 41.0 cc-mm/m²-24hr-atm | 104 cc-mil/100 in²-24hr-atm | or 1070 cc/m²-atm-24 hr per 38 µm film; 38°C; 90% RH Difference |
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin Film Properties.Data provided by the manufacturer. |