Polymer Property : Oxygen Transmission = 0.0780 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.0780 cc-mm/m²-24hr-atm
0.198 cc-mil/100 in²-24hr-atm
or 6 cc/m²-24hr-atm for the film. ASTM D3985
DuPont Teijin Films Mylar® M45 Polyester Film, 50 Gauge (15 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45..