Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 84 - 102 g/10 min @Load 21.6 kg, Temperature 190 °C |
84 - 102 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4133Q (33403) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 84 - 102 g/10 min @Load 21.6 kg, Temperature 190 °C |
84 - 102 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |