Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers SAN 290 Light Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |