Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 76 g/10 min @Load 5.00 kg, Temperature 200 °C |
76 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Melt Flow | 76 g/10 min @Load 10.0 kg, Temperature 220 °C |
76 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |