Physical Properties Metric English Comments
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Melt Flow 6.3 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.3 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE BU46-060 High Density Polyethylene Resin
Product Description: BU46-060 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt ..
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Melt Flow 6.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.