Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.1 g/10 min @Load 5.00 kg, Temperature 190 °C |
6.1 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |