Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 52.6 g/10 min @Load 5.00 kg, Temperature 230 °C |
52.6 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |