Melt Flow 52.53 g/10 min

@Load 8.70 kg,
Temperature 190 °C
52.53 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged..