Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB1501 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (480000 ppm) Features: Recyclable Material Uses: Compounding Forms: Pellets Processing Method: ..