Physical Properties Metric English Comments
Melt Flow 5.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 5.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.