Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 48 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® INP222 ABS
Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers.
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S701S ABS (Europe-Africa-Middle East)
CYCOLAC S701S is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appl..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycolac® S701S ABS (Europe-Africa-Middle East)
CYCOLAC S701S is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appl..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East)
CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East)
CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce..
Melt Flow 48 g/10 min

@Load 1.20 kg,
Temperature 300 °C
48 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East)
Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 200 °C
48 g/10 min

@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
Supreme Petrochem SP 6503 High Impact Polystyrene
Characteristics High Impact Available in various colors Easy flow High stiffness Processing Injection moldingApplications Computer cabinet, printer body, business machine housing etc. Material St..
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-765A ABS - Flame Retardant
F.R. High Flow
Melt Flow 48 g/10 min

@Load 10.0 kg,
Temperature 220 °C
48 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Copyright © lookpolymers.com All Rights Reserved