Polymer Property : Melt Flow = 45 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 35 - 45 g/10 min

@Load 21.6 kg,
Temperature 190 °C
35 - 45 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 50; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6348M (486F8) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 35 - 45 g/10 min

@Load 21.6 kg,
Temperature 190 °C
35 - 45 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 50; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6750H (506H8) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer