Polymer Property : Melt Flow = 41 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 41 g/10 min

@Load 5.00 kg,
Temperature 260 °C
41 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Melt Flow 41 g/10 min

@Load 5.00 kg,
Temperature 260 °C
41 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Melt Flow 41 g/10 min

@Load 5.00 kg,
Temperature 260 °C
41 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..