Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 38.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
38.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |