Physical Properties Metric English Comments
Melt Flow 31.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
31.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers SAN 290 High Flow Natural
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 31.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
31.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers SAN 300 Natural
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 31.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
31.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers SAN 300 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 31.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
31.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.