Polymer Property : Melt Flow = 30.9 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 30.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers Softflex® 0921
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.