Polymer Property : Melt Flow = 27.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 27.5 g/10 min

@Load 5.00 kg,
Temperature 230 °C
27.5 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis MD231U Polypropylene Compound, Mineral Filled
MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc..