Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
26.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 750 HF PLATABLE ABS/PC Alloy, Platable Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 26.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
26.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY ABSPC 750 HF ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 26.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
26.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |