Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 25.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
25.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 750 HF PLATABLE ABS/PC Alloy, Platable Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 25.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
25.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY ABSPC 750 HF ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |